Component polyethylene powder dosage
Preparation and Curing The polyethylene powder was sprinkled on the surface of the anodized aluminum part, and was lapped and cured at a pressure of 0.3-0.5 MPa and 200° C. for 1 hour.
Use The glue is mainly used for bonding of anodized aluminum products.